Preparation
1. Surfaces to be painted must be free of oil, dust grease, wax and old loosely adhering finish, cracking, and scaling paint.
2. All cracks and open joints should be sealed.
3. On new concrete surfaces apply SPHERO CONCRETE NEUTRALIZER while wood must be scuff sanded prior to paint application.
2. All cracks and open joints should be sealed.
3. On new concrete surfaces apply SPHERO CONCRETE NEUTRALIZER while wood must be scuff sanded prior to paint application.
application
FOR CONCRETE or WOOD.
1. Apply one (1) coat of SPHERO SPHERTEX PRIMER WHITE. Allow to dry for 4 hours.
2. For a Textured Finish, use a mortar or splatter gun, apply SPHERO SPHERCAST.
- Reduce to spraying consistency with SPHERO SPHERTEX REDUCER.
- Let dry for 5-10 minutes before flattenig the rough texture with a metal roller pre-wetted with water.
- Different textures are archieved depending on nozzle diameter opening and air pressure, the higher the air pressure , the smaller the texture size. For a bigger texture effect, lower the air pressure.
3. For a Plaing Finish, omit all application procedure for a Textured Finish and proceed to Topcoat Application.
4. Apply the topcoat, using a brush, roller or spray gun, apply 2 coats of white or colored SPHERO SPHERTEX GLOSS or SEMI-GLOSS.
1. Apply one (1) coat of SPHERO SPHERTEX PRIMER WHITE. Allow to dry for 4 hours.
2. For a Textured Finish, use a mortar or splatter gun, apply SPHERO SPHERCAST.
- Reduce to spraying consistency with SPHERO SPHERTEX REDUCER.
- Let dry for 5-10 minutes before flattenig the rough texture with a metal roller pre-wetted with water.
- Different textures are archieved depending on nozzle diameter opening and air pressure, the higher the air pressure , the smaller the texture size. For a bigger texture effect, lower the air pressure.
3. For a Plaing Finish, omit all application procedure for a Textured Finish and proceed to Topcoat Application.
4. Apply the topcoat, using a brush, roller or spray gun, apply 2 coats of white or colored SPHERO SPHERTEX GLOSS or SEMI-GLOSS.
preparation
1. Surfaces to be painted must be free of oil, dust grease, wax and old loosely adhering finish, cracking, and scaling paint.
2. All cracks and open joints should be sealed.
3. On new concrete surfaces apply SPHERO CONCRETE NEUTRALIZER while wood must be scuff sanded prior to paint application.
2. All cracks and open joints should be sealed.
3. On new concrete surfaces apply SPHERO CONCRETE NEUTRALIZER while wood must be scuff sanded prior to paint application.
Application
1. For Concrete Surfaces, apply one (1) coat of SPHERO FLAT LATEX WHITE or SPHERTEX PRIMER WHITE.
2. For Wood, apply SPHERO FLATWALL ENAMEL or SPHERO SPHERTEX PRIMER WHITE.
3. Using a standard roller spread SPHERO V-TEX TEXTURED PAINT at even thickness.
4. Using a pattern roller of choice, roll on lightly in one director with uniform pressure to impress desired texture effect.
5. As topcoat, apply one (1) coat SPHERO FLAT or SEMI-GLOSS or GLOSS LATEX WHITE.
preparation
1. Surfaces to be painted must be thoroughly cleaned and free of oil , dust, and grease, and wax, old loosely adhering finish, cracking and scaling paint by wiping, scraping and / or by sanding.
2. Ensure removal of grease and oil by use of solvent.
3. Surface must be thoroughly dry prior to primer application.
2. Ensure removal of grease and oil by use of solvent.
3. Surface must be thoroughly dry prior to primer application.
application
1. Apply by spray SPHERO LACQUER PRIMER enough to achieve ta dry film thickness of 1-1.5 mils / coat.
2. Sand properly primed surface to rid of surface roughness. Remove sand dust and other loose participles.
3. Apply SPHERO LACQUER GLAZING & SPOT PUTTY on wood surface imperfections such as open wood grains, nail heads, dents, scratches, shallow dents, etc. Touch dry in 15 minutes, sand in 1 hour. If necessary, recoat in 1 hour. If putty becomes stiff due to solvent evaporation, add small amount of SPHEOR LACQUER THINNER until ease o application is attained again.
4. Apply by spray SPHERO LACQUER Enamel. Touch dry in 10 minutes.
5. Recoat in 1 hour to achieve dry film, tichness of 1-1.5 mils/coat.
preparation
1. Surfaces to be painted must be thoroughly cleaned and free of oil , dust, and grease, and wax, old loosely adhering finish, cracking and scaling paint by wiping, scraping and / or by sanding.
2. Ensure removal of grease and oil by use of solvent.
3. Surface must be thoroughly dry prior to primer application.
2. Ensure removal of grease and oil by use of solvent.
3. Surface must be thoroughly dry prior to primer application.
APPLICATION
1. Reduce 1 part SPHERO LACQUER PRIMER to 1 part SPHERO LACQUER THINNER.
2. SPRAY SPHERO LACQUER PRIMER enough to achieve a dry film thickness of 1-1.5 mils/coat.
3. Sand properly primed surface to rid of surface roughness. Remove sand dust and other loose particles.
4. Using a putty knife apply SPHERO LACQUER GLAZING & SPOT PUTTY on wood surface imperfections such as open wood grains, nail heads, dents, scratches, shallow dents, etc.
- Touch dry in 15 minutes, sand in 1 hour. If necessarty, recoat in 1 hour. If putty becomes stiff due to solvent evaporation, add small amount of SPHERO LACQUER THINNER until ease of application is attained again.
5. Apply by spray SPHERO AUTOMOTIVE LACQUER. Touch dry in 10 minutes.
6. Recoat in 1 hour to achieve dry film thickness of 1-1.5 mils/coat.
2. SPRAY SPHERO LACQUER PRIMER enough to achieve a dry film thickness of 1-1.5 mils/coat.
3. Sand properly primed surface to rid of surface roughness. Remove sand dust and other loose particles.
4. Using a putty knife apply SPHERO LACQUER GLAZING & SPOT PUTTY on wood surface imperfections such as open wood grains, nail heads, dents, scratches, shallow dents, etc.
- Touch dry in 15 minutes, sand in 1 hour. If necessarty, recoat in 1 hour. If putty becomes stiff due to solvent evaporation, add small amount of SPHERO LACQUER THINNER until ease of application is attained again.
5. Apply by spray SPHERO AUTOMOTIVE LACQUER. Touch dry in 10 minutes.
6. Recoat in 1 hour to achieve dry film thickness of 1-1.5 mils/coat.
PREPARATION
1. Surfaces to be painted must be thoroughly cleaned and free of oil , dust, and grease, and wax, old loosely adhering finish, cracking and scaling paint by wiping, scraping and / or by sanding.
2. Ensure removal of grease and oil by use of solvent.
3. Surface must be thoroughly dry prior to primer application.
2. Ensure removal of grease and oil by use of solvent.
3. Surface must be thoroughly dry prior to primer application.
APPLICATION
SPHERO EPOXY PRIMER / ENAMEL
1. With brush, roller, or spray, apply 1 or 2 coats of SPHERO EPOXY PRIMER. If needed recoat after 6 hours.
2. As topcoat, apply 2 coats of SPHERO EPOXY ENAMEL, Chlorinated Rubber, Acrylic, or Lacquer paints. Touch dry in 1-2 hours, recoat in 4-6 hours. Hard Dry in 24 hours. Full cure in 7 days.
SPHERO EPOXY FLOOR COATING
1. With brush, roller, or spray , apply 1 or 2 coats of SPERO EPOXY FC SEALER.
2. As topcoat, apply 2 coats of SPHERO EPOXY FLOOR COATING. Recoat after 4-6 hours. Hard Dry in 24 hours. Full cure in 7 days.
SPHERO EPOXY SOLVENTLESS SL FINISH
1. With brush or roller, apply 1 or 2 coats of SPHERO EPOXY HD Sealer, for a Plain Floor Coat System.
2. As topcoat, apply 2 coats of SPHERO EPOXY SOLVENTLESS SL FINISH. Allow overnight intercoating interval. Hard Dry for light human traffic in 72 hours. Full cure in 7 days.
1. With brush, roller, or spray, apply 1 or 2 coats of SPHERO EPOXY PRIMER. If needed recoat after 6 hours.
2. As topcoat, apply 2 coats of SPHERO EPOXY ENAMEL, Chlorinated Rubber, Acrylic, or Lacquer paints. Touch dry in 1-2 hours, recoat in 4-6 hours. Hard Dry in 24 hours. Full cure in 7 days.
SPHERO EPOXY FLOOR COATING
1. With brush, roller, or spray , apply 1 or 2 coats of SPERO EPOXY FC SEALER.
2. As topcoat, apply 2 coats of SPHERO EPOXY FLOOR COATING. Recoat after 4-6 hours. Hard Dry in 24 hours. Full cure in 7 days.
SPHERO EPOXY SOLVENTLESS SL FINISH
1. With brush or roller, apply 1 or 2 coats of SPHERO EPOXY HD Sealer, for a Plain Floor Coat System.
2. As topcoat, apply 2 coats of SPHERO EPOXY SOLVENTLESS SL FINISH. Allow overnight intercoating interval. Hard Dry for light human traffic in 72 hours. Full cure in 7 days.